What is the difference between style CG and CGI spiral wound gaskets?
CG has an outer centring ring only. CGI adds an inner ring, which protects the windings from buckling inwards and keeps them out of the flow. ASME B16.20 calls for an inner ring with PTFE and flexible graphite fillers unless the purchaser specifies otherwise, so CGI is our standard for raised-face flanges.
When should I choose Kammprofile over spiral wound?
Choose Kammprofile for heat exchangers, joints with frequent thermal or pressure cycling, and flanges that cannot take high bolt load. Spiral wound is usually the economical choice for standard process pipework. The gasket selector compares them for your joint.
Can a spiral wound gasket be reused?
No. The windings deform permanently when the joint is tightened. Fit a new gasket every time the joint is opened.
What do the colours on the outer ring mean?
ASME B16.20 colour-codes the outer ring by winding metal (for example green for 316L, yellow for 304) and adds a stripe for the filler (grey for graphite, white for PTFE). See the colour code table.
Do you make non-standard sizes and shapes?
Yes. Spiral wound, Kammprofile and double jacketed gaskets are made to drawing in any diameter, including oval, obround and heat exchanger shapes with pass partitions.
Ordering
What information do you need for a quotation?
Size, pressure class, flange standard and face, gasket type, metal and filler, and quantity. For anything above 260 °C, give the design temperature and media. Drawings are needed for non-standard gaskets.
Can you kit gaskets for a shutdown?
Yes. We kit and label gaskets by joint or tag number so they reach the right flange. See shutdown service.
What certificates come with an order?
EN 10204 3.1 material certificates with every order, traceable to the strip, filler and ring material. Third-party witnessed inspection and 3.2 certificates are available on request.
What are your lead times?
Lead times depend on size, material and quantity, and are confirmed on every quotation. Urgent orders are prioritised for plant shutdowns.
Installation
How tight should I tighten the bolts?
Use the target bolt stress in your company procedure or ASME PCC-1. Our bolt torque calculator gives a starting torque and pass sequence for standard flanges.
Why do gasketed joints leak after start-up?
The most common causes are uneven bolt load, insufficient bolt load, damaged flange faces, re-used gaskets and the wrong filler for the temperature. Our article on gasket failures covers each.
Should I use paste or jointing compound on the gasket?
No. Do not apply compound or tape to spiral wound or Kammprofile gaskets. Lubricate the bolt threads and nut faces only.